Talk Composites - The Forum for Advanced Composites

Front Splitter

http://www.talkcomposites.com/Topic11758.aspx

By wozza - 6/10/2014 9:35:34 PM

The Fiesta St I have been making parts for doesn't have a splitter as standard, this one I made should be fitted to the car pretty soon. Lay up was  GC 50 - 2 x 450 CF - 10mm foam core - 2 x 450 CF using infusion.

Warren
By brainfart - 6/16/2014 3:54:06 PM

Or use a microballoons/resin mixture to fill the gap.