Trevor Harris
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 22,
Visits: 116
Hi All,
When using 'Biotex' 200g flax fibre 2/2 twill in carbon infusion, how many layers will give 1mm thickness after cure? Is there an advantage in using 400g and fewer layers in carbon or bio composites?How many layers will give 1mm finished thickness using 400g ?
Thanks
Trevor
Reply
Like
2
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
A general rule I go by is every 200g/sm is around .25-.3 mm thick when cured
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
2
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search