Biocomposites number of layers


Author
Message
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
A general rule I go by is every 200g/sm  is around .25-.3 mm thick when cured
Trevor Harris
Trevor Harris
Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)Supreme Being (159 reputation)
Group: Forum Members
Posts: 22, Visits: 116
Hi All,

            When using 'Biotex' 200g flax fibre 2/2 twill in carbon infusion, how many layers will give 1mm thickness after cure? Is there an advantage in using 400g and fewer layers in carbon or bio composites?How many layers will give 1mm finished thickness using 400g ?

Thanks

Trevor