By Trevor Harris - 6/3/2014 1:18:07 PM

Hi All,

            When using 'Biotex' 200g flax fibre 2/2 twill in carbon infusion, how many layers will give 1mm thickness after cure? Is there an advantage in using 400g and fewer layers in carbon or bio composites?How many layers will give 1mm finished thickness using 400g ?

Thanks

Trevor
By ajb100 - 6/3/2014 1:38:49 PM

A general rule I go by is every 200g/sm  is around .25-.3 mm thick when cured