Group: Forum Members
Posts: 680,
Visits: 1.9K
|
Hi Joe,
Definately not. This should be considered a flexible resin and should not be used for anything other than when a flexible (rubber-like) material is required/desired. The impact resistance would be better than a rigid resin but you would lose almost all of the structural strength. It's hard to explain, maybe we'll do a video which shows the cured properties of the system. Looking at the shore-hardness numbers alone seems to give the wrong impression. It's much more like rubber than a rigid resin. As such, most applications will be something different to normal laminating.
All the best, Matt
Matt Statham Easy Composites / Carbon Mods - Technical Sales
|