Shattered carbon exaust pipes


Author
Message
kylle
kylle
Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)
Group: Forum Members
Posts: 34, Visits: 101
Hi!

I have a shattered exhaust pipe from a Honda CBR. 

The chain broke and end up hitting the exhaust making a hole in the process...

What do I need to repair it... 
http://www.talkcomposites.com/Uploads/Images/0571e516-1d63-4541-a615-ce25.JPG
Reply
kylle
kylle
Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)Supreme Being (306 reputation)
Group: Forum Members
Posts: 34, Visits: 101
tanks;

but I tink I will disassembly the whole thing and start working from the inside. After renforcing the inside, i will do was U said in the outside but without the foam,... theres a big crack that isn't visible on the picture....