Shattered carbon exaust pipes
Shattered carbon exaust pipes
Post Reply
Like
4
Shattered carbon exaust pipes
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
kylle
kylle
posted 14 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 34,
Visits: 101
Hi!
I have a shattered exhaust pipe from a Honda CBR.
The chain broke and end up hitting the exhaust making a hole in the process...
What do I need to repair it...
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Shattered carbon exaust pipes
kylle
-
14 Years Ago
Hey Kylle, that looks like standard 200g 2/2 twill carbon to me, to repair it I woudl go to chop...
MAVERICK
-
14 Years Ago
It's not aaestheticallyrepair that I looking for. the repair patch doesn'tstayvisible....
kylle
-
14 Years Ago
well what i do when i repair an exaust is i lower the area where i want to add the carbon soi sand...
mhdghoul
-
14 Years Ago
tanks; but I tink I will disassembly the whole thing and start working from the inside. After...
kylle
-
14 Years Ago
Post Reply
Like
4
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search