Shattered carbon exaust pipes
http://www.talkcomposites.com/Topic955.aspx
By kylle
-
3/7/2012 12:01:17 AM
Hi!
I have a shattered exhaust pipe from a Honda CBR.
The chain broke and end up hitting the exhaust making a hole in the process...
What do I need to repair it...
By kylle
-
3/19/2012 12:00:38 AM
tanks;
but I tink I will disassembly the whole thing and start working from the inside. After renforcing the inside, i will do was U said in the outside but without the foam,... theres a big crack that isn't visible on the picture....