cressie
cressie
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 5,
Visits: 20
Is it possible to brush on the clear gel coat, as I have a large multi piece mould with overhanging flanges which make it impossible to spray on the gel coat?
As an alternative would it be possible to spray each part of the mould and while still wet carefully bolt it together?
Thanks!
Reply
Like
3
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Yes you can brush gel coat on, you just have to ensure it's not too think in places to cause visual distortion
Reply
Like
3
combustioncraig
combustioncraig
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 26,
Visits: 46
If your gel coat it epoxy based (few are) you can absolutely bush it on. It can be applied as thick as 2.5-3mm (it will be brittle) and can be done in multiple coats. If your gel coat is poly based (most are) then I believe you are shooting for a target thickness of .02 get a gel coat thickness gauge and be sure to degass the gel coat. Be sure to post pics of your project. Also I have found that foam brushes(make sure it won't melt the foam) provide a better results lease streaks than the typical nylon hair brush.
Reply
Like
3
20_rc51_00
20_rc51_00
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
How about brushing on with a semipermed mold with frekote semiperm? That stuff is so slick that I would be worried about the gelcoat balling up and forming droplets before it begins to tack..... any insight?
Edited
12 Years Ago by
20_rc51_00
Reply
Like
2
Brian_s
Brian_s
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 99,
Visits: 2.5K
After using a
chemical release agent add a coat or two of
Mould release
wax. It gives the Gel coat something to stick to.
Brian.
Reply
Like
2
Fasta
Fasta
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 468,
Visits: 3.5K
Brian_s (30/03/2014)
After using a
chemical release agent add a coat or two of
Mould release
wax. It gives the Gel coat something to stick to.
Brian.
I concur.
Fastacraft Facebook page
Reply
Like
2
20_rc51_00
20_rc51_00
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 95,
Visits: 548
Great! thanks
Reply
Like
3
bewbzout
bewbzout
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 16,
Visits: 46
Quick question, do you add wax after pva on all your molds or just ones explained above? Thanks
Reply
Like
3
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
The wax needs to go on before the pva, or the pva will be taken off. If your using a semi perm release agent then you wax second
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search