Talk Composites - The Forum for Advanced Composites

Brushing on the clear gel coat

http://www.talkcomposites.com/Topic9824.aspx

By cressie - 2/21/2014 12:51:16 PM

Is it possible to brush on the clear gel coat, as I have a large multi piece mould with overhanging flanges which make it impossible to spray on the gel coat?

As an alternative would it be possible to spray each part of the mould and while still wet carefully bolt it together?

Thanks!
By ajb100 - 4/21/2014 9:29:28 PM

The wax needs to go on before the pva, or the pva will be taken off. If your using a semi perm release agent then you wax second