Resin and Vacuum Line Plot -> Need Informed Opinions


Author
Message
turbodunn
turbodunn
Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)Forum Guru (71 reputation)
Group: Forum Members
Posts: 11, Visits: 94
I am pre-planning my infusion project and I am on the fence as to how to lay out my spiral tube for both the resin and vacuum lines. There is a lot going on with this mold so I want to be sure that the part wets out properly. I have made a few diagrams to share my thoughts and see if anyone else has an opinion.

Legend:

Green Line = Resin Spiral
Blue Line = Vacuum Spiral
Red Dot / Green Line = Resin Feed
Red Dot / Blue Line = Vacuum Feed

Plan A: Pull from one side to the other

[/URL]

Plan B: Pull vacuum from the center line of the part and run the resin along the perimeter

[/URL]


Does anyone have a take on which would work best or is there a better way about it?

-Jeff



Edited 12 Years Ago by turbodunn
Reply
Zorongo
Zorongo
Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)Supreme Being (276 reputation)
Group: Forum Members
Posts: 40, Visits: 330
OK, understood. Tjhanks !
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
turbodunn - 12 Years Ago
matthieutje65 - 12 Years Ago
baja_patient - 12 Years Ago
ChrisR - 12 Years Ago
Zorongo - 12 Years Ago
ChrisR - 12 Years Ago
turbodunn - 12 Years Ago
Zorongo - 12 Years Ago
baja_patient - 12 Years Ago
turbodunn - 12 Years Ago
baja_patient - 12 Years Ago
turbodunn - 12 Years Ago
turbodunn - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search