turbodunn
turbodunn
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 11,
Visits: 94
I am pre-planning my infusion project and I am on the fence as to how to lay out my spiral tube for both the resin and vacuum lines. There is a lot going on with this mold so I want to be sure that the part wets out properly. I have made a few diagrams to share my thoughts and see if anyone else has an opinion.
Legend:
Green Line = Resin Spiral
Blue Line = Vacuum Spiral
Red Dot / Green Line = Resin Feed
Red Dot / Blue Line = Vacuum Feed
Plan A: Pull from one side to the other
[/URL
]
Plan B: Pull vacuum from the center line of the part and run the resin along the perimeter
[/URL
]
Does anyone have a take on which would work best or is there a better way about it?
-Jeff
Edited
12 Years Ago by
turbodunn
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Resin and Vacuum Line Plot -> Need Informed Opinions
turbodunn
-
12 Years Ago
I always prefer to infuse from the center and draw a vacuum around...that way you have a strong/even...
matthieutje65
-
12 Years Ago
This is the perfect application for the MTI hose. Just lay some around the perimeter and have a...
baja_patient
-
12 Years Ago
I'd probably do something like B but without the vac line on the left and maybe finish the top and...
ChrisR
-
12 Years Ago
Hi Chris ! Just one question. (I have no experience with infusión, just thinking to start after many...
Zorongo
-
12 Years Ago
Bit of a rubbish image but shows what I mean. The hose you can see is the vac line. The peel ply...
ChrisR
-
12 Years Ago
Great input everyone! I really do appreciate it. It looks like it is plan B, with no spiral on the...
turbodunn
-
12 Years Ago
OK, understood. Tjhanks !
Zorongo
-
12 Years Ago
Hey Turbo, as I was saying, I like to slow my resin inlet (by slowly opening the resin clamp on the...
baja_patient
-
12 Years Ago
I just bought 30ft of MTI hose after taking a closer look. This hose looks to be the best thing to...
turbodunn
-
12 Years Ago
Excellent! I am sure you will love the results. Yeah I tend to mix a little more than needed,...
baja_patient
-
12 Years Ago
[quote][b]baja_patient (12/12/2013)[/b][hr]Excellent! I am sure you will love the results. Yeah I...
turbodunn
-
12 Years Ago
[quote][b]baja_patient (12/12/2013)[/b][hr]Excellent! I am sure you will love the results. Yeah I...
turbodunn
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search