Hi,
I have finally finished my first project. I thought I would start with something easy.
Brian.
Edited
12 Years Ago by
Brian_s
Reply
Like
7
Reply
fgayford
fgayford
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 433,
Visits: 1.2K
Brian_s (17/11/2013)
Hi,
I have finally finished my first project. I thought I would start with something easy.
Brian.
Nice job Brian, it looks great and I think it sounds vastly superior to the wooden one!
The big bonus with making instruments in carbon fiber is that the voice is so much more powerful and loud.
Our violins and guitar both had this positive effect.
Fred
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Harp
Brian_s
-
12 Years Ago
Hi! This part is AMAZING, looks awesome. I think this is a good example when hard work paid off. Can...
wojtepanik
-
12 Years Ago
Yes it is made to be played. It sounds great. My wife has a wooden one that this is based on. As the...
Brian_s
-
12 Years Ago
Stunning :) Is the tone any different compared to the original? Warren
wozza
-
12 Years Ago
Hey, Been a while I did not post, but now I feel like it's time to. This piece is awesome in...
Joe
-
12 Years Ago
Wow, that is stunning! Have you considered getting it pinstriped?
FLD
-
12 Years Ago
The tone is similar if not smoother and rounder. It also seems slightly louder. It is hard to...
Brian_s
-
12 Years Ago
Sound files. I hope this works. I have never used soundcloud before. Brian....
Brian_s
-
12 Years Ago
the wooden one sounds more mellow, the CF one sounds a little "bright" but that may mellow once...
ChrisR
-
12 Years Ago
Hats off to an awesome project!!! congrats, sounds great too, although im no expert. cheers
baja_patient
-
12 Years Ago
Thank you all for your kind words. Chris, I think the problem with the sound is that the start of...
Brian_s
-
12 Years Ago
[quote][b]Brian_s (17/11/2013)[/b][hr]Hi, I have finally finished my first project. I thought I...
fgayford
-
12 Years Ago
To my ear, the Carbon Harp sounds brighter and has much more "sustain" on the strings than the...
Dravis
-
12 Years Ago
Post Reply
Like
7
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search