Ive worked with the smc /bmc material that is being floated around as forged carbon. Ive used a few different types from quantum hexcel and another company. Its usually an epoxy resin system cured around 150 degrees. The thermoplastic sheets also known as organo sheets are usually pei or pps and require a forming temp of around 350degrees celsius. We use steel tooling for this as ali tools move about to much due to the expansion.
|