Hi, can anyone recommend a UV protective clear coat that I can use with vacuum only prepreg? Maybe one I can spray in mould? 
I want to kill 2 birds with 1 stone, pinholes and UV.
Any help is appreciated. Thanks.


http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
Reply
mawgan
mawgan
Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)
Group: Forum Members
Posts: 12, Visits: 32
A clear Vinylester skin coat can be used which gives you multiple application options including spraying directly to mould surface but this of course depends on what temperature you are curing at.