I second Cactus' question.  Can GC50 be used with prepreg?
mawgan
mawgan
Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)
Group: Forum Members
Posts: 12, Visits: 32
Forgot about this:

http://www.marineware.com/index.php?option=com_content&view=category&id=88:durepox-clear&Itemid=88&layout=default

Marineware are the UK distributors for Durepox and it is one of the best clearcoats you can use with epoxy composit components.
fgayford
fgayford
Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)Supreme Being (3.6K reputation)
Group: Forum Members
Posts: 433, Visits: 1.2K
carboncactus (16/05/2013)

Hi, can anyone recommend a UV protective clear coat that I can use with vacuum only prepreg? Maybe one I can spray in mould? 
I want to kill 2 birds with 1 stone, pinholes and UV.
Any help is appreciated. Thanks.



Hi
I often spray 2k automotive clear in my molds and then do a standard infusion the next day. Its important to leave it overnight. The 2 become one.
Its tricky to spray the clear to get it to lay down without beading but possible if you are not in a hurry. I have described my technic in detail some where on this forum.
Hope this helps.
Fred  

Greg
Greg
Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)Forum Guru (55 reputation)
Group: Forum Members
Posts: 7, Visits: 353
carboncactus (16/05/2013)
I want to kill 2 birds with 1 stone, pinholes and UV.
.

It's not possible you will get closed  air bubbles, but if you want try you can use polyurethane clear coat
Edited 12 Years Ago by Greg
mawgan
mawgan
Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)Supreme Being (104 reputation)
Group: Forum Members
Posts: 12, Visits: 32
A clear Vinylester skin coat can be used which gives you multiple application options including spraying directly to mould surface but this of course depends on what temperature you are curing at.
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K
Maybe someone from EC can tell me if their GC50 is compatible with Epoxy prepregs?

http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
carboncactus
carboncactus
Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)Supreme Being (1.8K reputation)
Group: Forum Members
Posts: 243, Visits: 1K

Hi, can anyone recommend a UV protective clear coat that I can use with vacuum only prepreg? Maybe one I can spray in mould? 
I want to kill 2 birds with 1 stone, pinholes and UV.
Any help is appreciated. Thanks.


http://www.talkcomposites.com/Uploads/Images/db628ad5-e0e7-47b9-873a-3d84.png
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search