Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pre-Pregs
»
UV clear coat
UV clear coat
Post Reply
Like
3
UV clear coat
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
carboncactus
carboncactus
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 243,
Visits: 1K
Hi, can anyone recommend a UV protective clear coat that I can use with vacuum only prepreg? Maybe one I can spray in mould?
I want to kill 2 birds with 1 stone, pinholes and UV.
Any help is appreciated. Thanks.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
UV clear coat
carboncactus
-
12 Years Ago
Maybe someone from EC can tell me if their GC50 is compatible with Epoxy prepregs?
carboncactus
-
12 Years Ago
A clear Vinylester skin coat can be used which gives you multiple application options including...
mawgan
-
12 Years Ago
[quote][b]carboncactus (16/05/2013)[/b][hr] I want to kill 2 birds with 1 stone, pinholes and UV. ....
Greg
-
12 Years Ago
[quote][b]carboncactus (16/05/2013)[/b][hr] Hi, can anyone recommend a UV protective clear coat...
fgayford
-
12 Years Ago
Forgot about this:...
mawgan
-
12 Years Ago
I second Cactus' question. Can GC50 be used with prepreg?
cpkielycua
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search