This is an upper section/tacho mount for a classic race bike, the original part in glass fibre weighs 350 grams and the carbon component is 80 grams. I used wet lay and vacuum  bag. I will be making a complete fairing later this week for the same bike .



http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Replies
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Chris, looks like a nice project. Can I ask why your not using Infusion as it sounds like you have a vac pump?

Warren

Carbon Copies Ltd
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Warren

Yes i have a pump and all the items req ie spiral tube, why not use them ? a good question, i have had some good results using wet lay and vacuum bag and most the parts i make are  for go and not show and the race bodywork will be painted. I do feel tempted to use it on the next fairing . what is the current situation with suitable spray adhesives to hold the layers of cloth on place ? i may become a convert Smile

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
Edited 12 Years Ago by Bartonphoenix750
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
matthieutje65 - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
Chris - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
wozza - 12 Years Ago
carbonfibreworks - 12 Years Ago
Chris - 12 Years Ago
carbonfibreworks - 12 Years Ago
Warren (Staff) - 12 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search