Vinylester/CSM moulds...


Author
Message
GROPIUS
GROPIUS
Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)
Group: Forum Members
Posts: 13, Visits: 332
Hi there
I recently made some moulds made out of Vinylester/CSM.
The gel coat is Polyester based.
So now the question is...
...how long do I have to wait until I'll be able to use the moulds to build composite parts?

Btw...
...I'll be using ECs GC50 gel coat combined with epoxy resin on the composite parts.

Reply
wozza
wozza
Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)Supreme Being (4.9K reputation)
Group: Forum Members
Posts: 688, Visits: 5.4K
Hi Fred, it lays down really well with no beading or fish eyeing. The first time I used it I was really worried by the slight orange peel finish it has when sprayed. But once infused or even wet laid the part comes out like glass.Smile 

Warren

Carbon Copies Ltd
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
GROPIUS - 12 Years Ago
fgayford - 12 Years Ago
GROPIUS - 12 Years Ago
matthieutje65 - 12 Years Ago
alebassa - 12 Years Ago
GROPIUS - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
GROPIUS - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
fgayford - 12 Years Ago
GROPIUS - 12 Years Ago
GROPIUS - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Ozonedge - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search