Vinylester/CSM moulds...


Author
Message
GROPIUS
GROPIUS
Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)
Group: Forum Members
Posts: 13, Visits: 332
Hi there
I recently made some moulds made out of Vinylester/CSM.
The gel coat is Polyester based.
So now the question is...
...how long do I have to wait until I'll be able to use the moulds to build composite parts?

Btw...
...I'll be using ECs GC50 gel coat combined with epoxy resin on the composite parts.

Replies
GROPIUS
GROPIUS
Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)Supreme Being (83 reputation)
Group: Forum Members
Posts: 13, Visits: 332
fgayford (29/03/2013)
If you are at room temperature a few days will do it.

Just a suggestion from years of experience, do your self a favor and use EasyLease instead of the wax PVA route as a release agent.

Wax and PVA still have their place but its just so barbaric compared to the new chemical release agents.

I wonder what I have been doing all these years with wax and PVA.

My opinion!

Fred
Cheers Fred,
that sound promising.

Would post-curing speed up the process?

and...
...got my EasyLease delivered with the GC50Wink 
Matthieu Libeert
Matthieu Libeert
Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)Supreme Being (7.5K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
Yes it will, you need to get the styrene out of the mould and by applying heat you will smell the styrene meaning it is being removed from the mould Smile

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
GROPIUS - 12 Years Ago
fgayford - 12 Years Ago
GROPIUS - 12 Years Ago
matthieutje65 - 12 Years Ago
alebassa - 12 Years Ago
GROPIUS - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
GROPIUS - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
fgayford - 12 Years Ago
wozza - 12 Years Ago
fgayford - 12 Years Ago
GROPIUS - 12 Years Ago
GROPIUS - 12 Years Ago
wozza - 12 Years Ago
wozza - 12 Years Ago
Jess8bit - 12 Years Ago
Ozonedge - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search