Hi,

I've seen videos where somebody creates a simple formwork around the front edge an old kitchen worktop and pours clear or pigmented epoxy resin over the worktop up to an inch or so, popping small surface bubbles with a blow torch and quickly transforming it into a beautiful glass-like surface with no unsightly carpentry joins. Question is:

1. What's the best epoxy for this? I'm thinking 'coating resin'?
2. Providing it's level, is this as easy as it looks or will I be entering a world of pain?

Thanks for your help.

Regards, James Hewings
Reply
Warren (Staff)
Warren (Staff)
Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)Supreme Being (22K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As yet, we don't stock a specific table top/worktop coating resin.  We have resins that are similar for skinning, but they have not been specially formulated or tested to see how well they would work as a coating for table tops/worktops.  As such we wouldn't want to recommend you something that might not perform as you would wish.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search