We are currently researching a supplier for a suitable table top type resin as we get a LOT of enquiries about such resins now.  Such resins are a lot harder to find than even we thought but we are making progress and hopefully will have something in the next few months if our research goes to plan.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
gopfem
gopfem
Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)Forum Member (35 reputation)
Group: Forum Members
Posts: 1, Visits: 3
I am sharing the dilemma you shared last year. Would you be able to say where it got you to?
JamesH
JamesH
Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)
Group: Forum Members
Posts: 2, Visits: 64
Thanks for your advice. I've bought some coating resin and some laminating resin and I'm going to do some tests.
Warren (Staff)
Warren (Staff)
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
As yet, we don't stock a specific table top/worktop coating resin.  We have resins that are similar for skinning, but they have not been specially formulated or tested to see how well they would work as a coating for table tops/worktops.  As such we wouldn't want to recommend you something that might not perform as you would wish.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Matthieu Libeert
Matthieu Libeert
Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)Supreme Being (11K reputation)
Group: Forum Members
Posts: 955, Visits: 3.4K
There are some special resins for this kind of things,... some staff member can probably help you further.
Leveling it shouldn't be that difficult I guess, use some tools to level the surface

Matthieu Libeert
Founder MAT2 Composites X Sports
website:
www.mat2composites.com




JamesH
JamesH
Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)Forum Guru (68 reputation)
Group: Forum Members
Posts: 2, Visits: 64
Hi,

I've seen videos where somebody creates a simple formwork around the front edge an old kitchen worktop and pours clear or pigmented epoxy resin over the worktop up to an inch or so, popping small surface bubbles with a blow torch and quickly transforming it into a beautiful glass-like surface with no unsightly carpentry joins. Question is:

1. What's the best epoxy for this? I'm thinking 'coating resin'?
2. Providing it's level, is this as easy as it looks or will I be entering a world of pain?

Thanks for your help.

Regards, James Hewings