Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
mold and release system
mold and release system
Post Reply
Like
3
mold and release system
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
tha_pop
tha_pop
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 17,
Visits: 877
quick question for you guys. What resin/gelcoat system are you using on your made of polyester gelcoat? i have made a mold for a mirror part using polyester system but the problem i'm having is that i'm using epoxy for the infusion and my part always get stuck on the mold no matter how much i wax the mold. with the last part i puller from the same mold i applied pva and again there was a bit if sticking but the finishing on the part was not that great
what are you using for ur release system maybe if you could outline the product and the steps it will be really great.
thanks in advance.
Reply
Like
3
Reply
ajb100
ajb100
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 346,
Visits: 4.4K
Uni mould is good but exPensive for one off's
With my polyester moulds, I leave them for a week befor eyeing and then a couple of coats of easy lease and a couple of coats of wax and they normally release fine, sometimes need to do a little bit of repair to the gel coat but nothing major
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
mold and release system
tha_pop
-
12 Years Ago
I use the Uni mold system and easy lease (spelling) with no issues even with a complex shape, i am...
carbonfibreworks
-
12 Years Ago
I use polyester gel coat, and also epoxy gel coat. I do piece with hand layup with polyester resin...
_GABBER
-
12 Years Ago
Uni-Mould then Easy Lease. All my work is Infusion and after 5/6 applications of Easy Lease on a new...
wozza
-
12 Years Ago
Uni mould is good but exPensive for one off's With my polyester moulds, I leave them for a week...
ajb100
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search