Hi

What's the (nominal) thickness of the pre-formed tapes - the same as 2/2 195g cloth (.28mm)?

Looking at custom bicycle 'guards, so want an arc of circa 850mm length by 25mm width on a 280mm radius,  but the clearance between tyre and frame is ~1.5mm, so there's not a lot of room for multiple layers...
Reply
20130218ec
20130218ec
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 4, Visits: 10
Shouldn't be too bad, as it's linear arc.

QUICK QUESTION: The heat shrink tape - can't see any indication of whether it's interior or exterior face (with respect to a presented roll) that should be applied to epoxy layer, i.e. there's no adhesive on either side of tape - if this is so I take it either way up is OK, before applying heat...
Edited 12 Years Ago by 20130218ec
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search