Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Any practice ideas.
Any practice ideas.
Post Reply
Like
3
Any practice ideas.
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Sharper
Sharper
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 6,
Visits: 35
I have just had everything delivered to do resin infusion. I have made my mould, and am pretty much ready to go.
I am fairly nervous about making the 1st one. Does anybody have any tips on doing some kind of practice run?
The carbon material is rather expensive, and I was toying with the idea of using some other kind of fabric for a practice run, would this work the same?
(
|
|):::::::
o
: (||[[(
(
)))))))))))))))))))))))))))))))))))))))))))))))))))))))))))))
)
Reply
Like
3
Reply
alebassa
alebassa
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 48,
Visits: 171
baja_patient (11/03/2013)
That is the nice thing about infusion. There is really no rush involved in the initial stages. You can really take your time doing the layup properly and making sure you have a 100% sealed bag. Once you are happy (it can take several hours and possibly a few vacuum bags when you are first starting out), then go ahead and carefully mix and degas resin, then infuse at the correct pace.
Planning and preparation make a big difference in your outcome.
cheers
That's really true... from my very little experience wet layup is really a mess and stressing experience if compared to infusion!
Alessandro
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Any practice ideas.
Sharper
-
12 Years Ago
Hi Sharper Why not just follow Matt's instruction video on making a hood scoop. Instead of a mold...
fgayford
-
12 Years Ago
If I'm making something big and unknown, I do a trial run with woven glass the same spec as the...
ajb100
-
12 Years Ago
OK, so i did a practice run, and wow I'm glad that I did. I'd have mucked it up big time. Basically,...
Sharper
-
12 Years Ago
You can also use polyester infusion resin to reduce the cost more but you can't really use it to...
ajb100
-
12 Years Ago
i think for my first few pieces, i will use FG first part. the 2nd maybe use polyester and CF for...
brasco
-
12 Years Ago
That is the nice thing about infusion. There is really no rush involved in the initial stages. You...
baja_patient
-
12 Years Ago
[quote][b]baja_patient (11/03/2013)[/b][hr]That is the nice thing about infusion. There is really no...
alebassa
-
12 Years Ago
Practicing with woven glass is a good idea as its a fraction of the cost of carbon.
Warren (Staff)
-
12 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search