Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Lantor Soric Core
Lantor Soric Core
Post Reply
Like
5
Lantor Soric Core
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
AlpineCoupe
A
AlpineCoupe
posted 5 Years Ago
ANSWER
HOT
Topic Details
A
Group: Forum Members
Posts: 45,
Visits: 2.1K
Hi all, I'm going to be making a flat carbon fiber practice panel with a 2 mm soric tf core and I'm wondering if it is necessary to chamfer the edge like I've seen in some literature? Going to be using a standard 2x2 twill weave to cover the core.
The chamfering seems common with more solid foam cores but just wanted to check before I finalize my plan. Thanks!
Reply
Like
5
Reply
oekmont
oekmont
posted 5 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 550,
Visits: 27K
Soric tf doesn't have flow channels. To chamfer soric I just cut it with a very sharp knife at a steep angle.
Reply
Like
6
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Lantor Soric Core
AlpineCoupe
-
5 Years Ago
If it's a part with cosmetic clear carbon surface, yes. Soric core leaves a visible edge on the surface, chamfering the core reduces it significantly. but with thin skin layups it's hard to avoid...
oekmont
-
5 Years Ago
It's also difficult to chamfer Soric nicely, it tends to tear too easily. It's also somewhat pointless given the flow channels will print just as much as the unchamfered edge will. Its easier to but...
Hanaldo
-
5 Years Ago
Soric tf doesn't have flow channels. To chamfer soric I just cut it with a very sharp knife at a steep angle.
oekmont
-
5 Years Ago
Ah of course, I missed that it was the TF version. Much better product, although still extremely heavy. I still feel any Soric core isn't worth chamfering. It's better and easier to build up the...
Hanaldo
-
5 Years Ago
I'm making the panel over sized and plan to trim it back to my specific dimensions so ultimately the chamfered edge in question is going to be cut off. Does that change the recommendations for or...
AlpineCoupe
-
5 Years Ago
Yes. Don't bother with chamfering. This is only a cosmetic issue
oekmont
-
5 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search