Thanks for the advice buddy! I think a 2 piece mould would be the way forward and I see what you mean about getting cloth in every section, wet lay and vaccum sounds a good idea I may have to try both techniques just to see what diffrence I get I can see it’s going to be a task and a half! But I think with patience and lots and lots of practice it will look a nice item! The part that stands vertical at the very front won’t be visible as it’s hidden by the numberplate but that doesn’t mean it can’t be a poor job, I’m hoping to have the underside lip reinforced with some Kevlar as it will get scraped badly with speed bumps. Yes West Yorkshire Leeds area abit far to travel to Essex unfortunately but thanks for the offer
|