Looking into pre preg.

Can any tell me roughly the full cost per sqm for using out of autoclave xpreg carbon? All layers needed including bagging materials etc..

And then cost of clear coating.

Cost of running the oven (easy composites)

Just trying to gauge the average cost of 1 small part made say wing mirror cover size.

Thanks
Reply
Hanaldo
Hanaldo
Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)Supreme Being (32K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
If you're using X-Preg, then no, not essential. Does always help though.