How do you make your sand blocks?


Author
Message
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Hi, what do you use as sand blocks for fairing?
I watched some tutorials but they were all about wood working. Wonder if there is some adjustment specific for composites.
So...
Wood (btw, with or without pads)?
Foam? Xps would be ok
Commercial available? Ifound permagrit blocks fantastic but they only make the coarser grits.

Thanks
Reply
Massimiliano
M
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 167, Visits: 1.1K
Chris Rogers - 5/22/2020 6:02:13 PM
You can also cast-in-place sanding blocks with some packing tape on your surface, some polyester filler (Bondo) to take the surface shape and a wood backer to hold on to...

I'm a big fan of the 3M yellow foam blocks and the Stickit paper too - the blocks are hard enough yet have some give.  Not cheap but a great system.

You can also glue acrylic sheet to softer foam to make a flexible-yet-hard block for curved surfaces.  You want to sand (fair) with something that takes the shape of the surface you want to achieve - but no more - so you hit the high spots but don't over-sand the low ones.

Lot of ideas, thank you!

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
mporta71 - 5 Years Ago
Hanaldo - 5 Years Ago
             Thanks a lot!!
mporta71 - 5 Years Ago
Warren (Staff) - 5 Years Ago
             Thank you!
mporta71 - 5 Years Ago
scottracing - 5 Years Ago
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
mporta71 - 5 Years Ago
SleepingAwake - 5 Years Ago
                     Thank you, I will have a look at them!
mporta71 - 5 Years Ago
explorecomposites - 5 Years Ago
             Lot of ideas, thank you!
mporta71 - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search