Hello everyone.
I know that if I lay carbon fibre on to aluminium I should either use glass fibre between the two materials, or possibly have the ally part anodised. Is the same true for using CF and mild steel? I have looked but cant seem to find any info for this situation.
Thanks for any advice.

JK
Reply
Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
oekmont - 1/11/2020 5:45:25 AM
In my experience this works best if the aluminium is "hard anodized" which is a thicker, more durable oxide layer, compared to regular (coloured) anodization.

Interesting point. Have you had issues with galvanic corrosion on regular anodized aluminium? 

I have bonded to both, and don't notice a difference, though I would agree that hard anodized is better in theory simply because it can be tricky to nicely prep a part without removing a coating less than 0.002mm thick... These days I don't actually bother, I don't like to include ali in the layup and prefer to do secondary bonding with a decent bond gap and sidestep CTE issues that may present themselves. 

Edited 5 Years Ago by Hanaldo
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
jaykay - 6 Years Ago
oekmont - 6 Years Ago
jaykay - 6 Years Ago
jaykay - 5 Years Ago
Hanaldo - 5 Years Ago
oekmont - 5 Years Ago
Hanaldo - 5 Years Ago
Fasta - 5 Years Ago
SleepingAwake - 5 Years Ago
Warren (Staff) - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search