Hello everyone.
I know that if I lay carbon fibre on to aluminium I should either use glass fibre between the two materials, or possibly have the ally part anodised. Is the same true for using CF and mild steel? I have looked but cant seem to find any info for this situation.
Thanks for any advice.

JK
Replies
jaykay
j
Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)Forum Guru (50 reputation)
Group: Forum Members
Posts: 6, Visits: 84
oekmont - 12/21/2019 7:43:55 AM
Yes. Even stainless steel.

Just a thought. If I were laying up onto Aluminium, could I get the aluminium anodised, would that also serve as a barrier against corrosion? 

Many thanks
JK

Hanaldo
Hanaldo
Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)Supreme Being (21K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
jaykay - 1/10/2020 11:02:42 AM
oekmont - 12/21/2019 7:43:55 AM
Yes. Even stainless steel.

Just a thought. If I were laying up onto Aluminium, could I get the aluminium anodised, would that also serve as a barrier against corrosion? 

Many thanks
JK

Yes. Just be sure to prep well, without removing the anodized surface. 

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
jaykay - 6 Years Ago
oekmont - 6 Years Ago
jaykay - 6 Years Ago
jaykay - 5 Years Ago
Hanaldo - 5 Years Ago
oekmont - 5 Years Ago
Hanaldo - 5 Years Ago
Fasta - 5 Years Ago
SleepingAwake - 5 Years Ago
Warren (Staff) - 5 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search