			            Or perhaps just go from side to side? Looks like your mould is only 50cm's across, so this feels like the most direct route. 
 Given the relative width, in this orientation, you'd just need to ensure that the outer edges don't lag too far behind the central area.
 
 Infusion spiral right along the inlet side, a resin break with a touch more gap in the centre to slow it up a little more here and, perhaps, an additional layer of infusion mesh at the outer edges. This should help to ensure that you're not left waiting for the outer edges to infuse when the resin reaches the exit port, as the extra layer will help speed things up here.
 
 As Hanaldo said, using a conventional silicone-type connector placed directly on the laminate is likely to leave some print through, so might blight the end result a bit
 
 |