		| By 8900120dd - 10/10/2019 2:14:59 PM 
 hi guys, ive finished making a large mould, however im not sure where would the best location to put the resin and vac pipes.
 im planning to put a vac pipe on each side of the mould and resin feed in the middle, but im worried the resin might not be able to climb up a 1m long roughly 70degree slope on each side.
 
 i have attached a picture to roughly illustrate the size of my mould.
 
 would like some input on where would be the best locations to put resin feed and vac pipes
   
 thanks
   |  
		| By Hanaldo - 10/12/2019 6:29:32 AM 
 Bang on Mark, I didn't even notice that measurement on the side and was imagining like a boat hull or something.
 
 I'd go side to side exactly as Mark described if it is only 50cm across.
 
 |  |