hi guys, ive finished making a large mould, however im not sure where would the best location to put the resin and vac pipes.
im planning to put a vac pipe on each side of the mould and resin feed in the middle, but im worried the resin might not be able to climb up a 1m long roughly 70degree slope on each side.

i have attached a picture to roughly illustrate the size of my mould.

would like some input on where would be the best locations to put resin feed and vac pipes Smile

thanks