Im getting minor bridging around the base of the raised areas (see pic) 

Do any of you guys think it is possible to get everything down into the tight corner?

   

   


Reply
Steve Broad
Steve Broad
Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)Supreme Being (3.4K reputation)
Group: Forum Members
Posts: 408, Visits: 4.1K
I am certainly no expert, but this looks so close. What weave and weight are you using? I ask this as different weaves have different drape characteristics. Also, a lighter cloth will drape easier, so maybe more layers of lighter material?

I await being corrected by oakmont and hanaldo :-)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search