By Darren - 11/6/2018 10:04:13 PM
Im getting minor bridging around the base of the raised areas (see pic)
Do any of you guys think it is possible to get everything down into the tight corner?


|
By oekmont - 11/8/2018 2:58:24 AM
An other option might be to lay down the cloth slightly diagonal, that there are no bumps along the fibre directions.
|
|