Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Resin Infusion
»
Minor Bridging
Minor Bridging
Post Reply
Like
3
Minor Bridging
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
Darren
Darren
posted 7 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 54,
Visits: 916
Im getting minor bridging around the base of the raised areas (see pic)
Do any of you guys think it is possible to get everything down into the tight corner?
Reply
Like
3
Reply
Hanaldo
Hanaldo
posted 7 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
Definitely possible. Easier with pre-preg, but certainly not impossible with infusion. You're very very close.
Reply
Like
2
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Minor Bridging
Darren
-
7 Years Ago
Definitely possible. Easier with pre-preg, but certainly not impossible with infusion. You're very very close.
Hanaldo
-
7 Years Ago
It could be done without cutting the fabric, but the fibre alignment would look nicer if you cut out the bumps and cover them with small circular pieces. That way, it would be much easier to avoid...
oekmont
-
7 Years Ago
I am certainly no expert, but this looks so close. What weave and weight are you using? I ask this as different weaves have different drape characteristics. Also, a lighter cloth will drape easier, s...
Steve Broad
-
7 Years Ago
One problem I see here, is that two of the bumps are in line with one of the fibre directions. So if you are trying to work on the bridging of one bump, you pull on the other. Better drape...
oekmont
-
7 Years Ago
As I paint my carbon alignment wouldn't be an issue for me, but I take your point. :-)
Steve Broad
-
7 Years Ago
This is exactly the issue I'm having. Im pushing into the corner of one bump and can see it pulling away from the other. I think I'm going to cut circles out where the bumps are and try that
Darren
-
7 Years Ago
An other option might be to lay down the cloth slightly diagonal, that there are no bumps along the fibre directions.
oekmont
-
7 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search