+x Hanaldo - 8/3/2018 10:24:16 PMThis will cause interlaminar bond issues ^ There are tapes made specifically for this like Airtech Airhold, but they are expensive and not really that useful.The 'web-lock' brand of set-weave carbon you can get from Composite Envisions. I've heard good things about it compared to other set-weave fabrics, and it's like the Toray version - much softer than the others and uses a hot melt binder rather than the b-staged epoxy.You don't really need it though, and you don't need an especially flexible fabric to tack to the back of your carbon, just tack two layers of carbon together. If you need more drape or conformability, cut the second layer so that the fibres are at 45 degrees - I find this is very rarely necessary.