resin leaks during infusion


Author
Message
suman
s
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 11, Visits: 79
I am infusing ly556  resin and hy951 hardener with glass fibres to produce laminates of size 300mmx 150mm with 2 mm thickness. problem is as soon i open the resin line for infusion, resin accumulates around the line ad leaks out between bagging tape and vacuum bag. please help to resolve this problem
Reply
suman
s
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 11, Visits: 79
oekmont - 6/19/2018 2:08:26 PM
Could it be, that the bag is just damaged by the stretched spiral? Spirals usually have quite sharp edges. Some vacuum bagging films can easily be damaged by these.
try to simply plug the resin hose into one end of the spiral. This perpendicular connection isn't nearly as smart as it seems at first glance. The resin flows so much faster through the spiral than through the flow mesh, that the resin front isn't affected much by the asymmetric setup.

I will try your suggestion and let you know the results

GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
suman - 7 Years Ago
oekmont - 7 Years Ago
oekmont - 7 Years Ago
Warren (Staff) - 7 Years Ago
suman - 7 Years Ago
oekmont - 7 Years Ago
suman - 7 Years Ago
suman - 7 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search