bonding metal to composites


Author
Message
suman
s
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 11, Visits: 79
hi, 
 i am trying to attach hinges to carbon composite for Double Cantilever Beam specimen using adhesive. lot of them are failing. Please suggest any alternate ways
Reply
Fasta
Fasta
Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)Supreme Being (4K reputation)
Group: Forum Members
Posts: 468, Visits: 3.5K
You could consider using a methacrylate adhesive like Plexus.
I find these work really well for metal to composite bonding.