hi, 
 i am trying to attach hinges to carbon composite for Double Cantilever Beam specimen using adhesive. lot of them are failing. Please suggest any alternate ways
Reply
suman
s
Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)Supreme Being (78 reputation)
Group: Forum Members
Posts: 11, Visits: 79
polaraligned - 11/14/2017 11:39:23 AM
What metal is the hinges made out of? 

hi,
my hinges are presently made of brass. i am using them as stainless steel hinges often failed due to poor adhesion. 