Hi!
Did you use GC50 before laying down the CF cloth, then infuse ? To me that looks like lumps of GC50 or other "in mould coating" -- The "milky look" does not look like normal bridging.
"Sapere Aude"... Dare to KNOW!
The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...
103% of all people do not understand statistics...
Do not adjust our mind, theres a fault in reality :-)
|