Hi  all  I am new here  I am try  make some carbon 
Fiber vents but  having no joy  I have tried 200gm
2x2 twill non weave set   And tryed 2x2. Twill 200gm weave 
Set  any info I would. Appreciate 
 Thanks graham 
Attachments
IMG_3678.JPG (432 views, 26.00 KB)
Reply
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
do you have any pictures? it sounds like you have bridging of the material? you need to ensure that prior to vacuum bagging and curing that the material is in all the female corners.