Hi all new here looking for help


Author
Message
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
The picture in my first post I made a mould off the top face  is that the right way to do 
Also when I put the carbon into the mould would I need to cut the slots in the carbon  for it to pull in better 
I appreciate any info thanks 
scottracing
scottracing
Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)Supreme Being (3.9K reputation)
Group: Forum Members
Posts: 460, Visits: 5.2K
do you have any pictures? it sounds like you have bridging of the material? you need to ensure that prior to vacuum bagging and curing that the material is in all the female corners.
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Yeh I made a mould   And I used pre preg 200gms non weave set and I tried 200grm weave set   Do I need to use a heavier  carbon  like 245 grm non weve set to get it to pull in tighter 
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
I'm not sure i quite follow you here?

Are you trying to "skin" these vents with 200gsm Twill?

OR:  Have you made moulds from them .. to wet lay or infuse them in CF 200 gsm ..

Pictures of the items that "went wrong" will tell us much more  ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Coxo
Coxo
Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)Supreme Being (399 reputation)
Group: Forum Members
Posts: 39, Visits: 476
Hi  all  I am new here  I am try  make some carbon 
Fiber vents but  having no joy  I have tried 200gm
2x2 twill non weave set   And tryed 2x2. Twill 200gm weave 
Set  any info I would. Appreciate 
 Thanks graham 
Attachments
IMG_3678.JPG (422 views, 26.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search