Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Pattern and Plug Making
»
Plug issues
Plug issues
Post Reply
Like
3
Plug issues
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
67redrocket
67redrocket
posted 9 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
I made a unimold of a plug today. The plug got bad and also the mold. Does anyone know what can have caused these problems? I have use both the pattern coat primer and the hi gloss on a MDF pattern.
Reply
Like
3
Reply
VVS
VVS
posted 9 Years Ago
ANSWER
HOT
Post Details
Group: Moderators
Posts: 226,
Visits: 334
i always leave the metal seal in the tin and make a small hole in one side so you only get a trickle coming out.
Reply
Like
4
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Plug issues
67redrocket
-
9 Years Ago
Looks like a release problem. I assume you are using Easylease? How did you apply it, how old is it?...
Hanaldo
-
9 Years Ago
Yes I used a 8 month old easy lease. Applyed it with a cloth six times like I always do. 15 minutes...
67redrocket
-
9 Years Ago
It sounds like this was definitely a release failure. How well did you clean the plug before...
Hanaldo
-
9 Years Ago
i always leave the metal seal in the tin and make a small hole in one side so you only get a trickle...
VVS
-
9 Years Ago
The problem can be: 1. Temperature at your workplace (most separators needs >25 C temperature...
ArturK
-
9 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search