Hi!

When molding carbon parts with high Vf (>50%) the fibres touching the mold are leaving a residue on my mold surface. I don't know why this is happening. I just bought easy lease release agent, but it also happened with wax (Partall). In fact I thought the Partall wax had aged so I bought Easy Lease thanks to this forum. But unfortunately no difference. The parts are demolding easy though with easy lease.

I have been using different curing processes: 24h room temp, 48h room temp, 24h 30 degrees C, 48h 30 degrees C. All with the same outcome: a residue on the mold. The molds are machined of PU toolingboard (Renshape) and polished to a mirror surface. Epoxies used are L + GL2 / S / L and EPH161 from R&G. When making a hand layup of one ply of carbon without compaction there is no printthrough and also no residue on the mold surface after demolding just like when using a gelcoat prior to the lay up.  So it looks like the problem is related to the compaction of the fibre or it maybe an epoxy problem.

In the video of the small bonnet Easycomposites doesn't use a gelcoat either. Is there also a residue left on the mold? Or is this problem related to the used epoxy? I don't mind a little print through on the part but the problem is that I have to repolish the mold and re apply the easy lease which eliminates the advantage of a semi perm.


Reply
seense
seense
Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)Supreme Being (117 reputation)
Group: Forum Members
Posts: 10, Visits: 138
Thanks! Appreciating every input and experience. Semi perms and RTM are new to me. After the last test I am also doubting if a lack of sealer is the problem. Maybe it's just about film thickness/strenght for this type of process. Although I thought one would have to apply multiple coats to ensure complete coverage. Or I don't understand how a semi perm works.

After demolding the last part I also noticed tape is sticking pretty bad again. So I guess I have to add multiple EL coats again. Wondering where all that release agent went because the part came out clean.