How do I fix this mould?


Author
Message
carbonfibreworks
carbonfibreworks
Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)Supreme Being (2.2K reputation)
Group: Forum Members
Posts: 292, Visits: 4.5K
Hi Redrocket
You can mix some gel coat and use it to fill the voids then flat back with some fine paper and polish and you should be able to remove the release tape with a sharp blade/ scalpel  .
Regards Chris  

http://www.talkcomposites.com/Uploads/Images/97e08777-693c-4af1-a27a-86cf.png
67redrocket
67redrocket
Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)Supreme Being (415 reputation)
Group: Forum Members
Posts: 49, Visits: 486
Made my second mould yesterday, but it did not turn out as good as the first one.

Is this mould fixable? 

How do I fix the bubble holes? And how do I get the release tape out of the mould?

http://www.talkcomposites.com/Uploads/Images/d4faf592-c2aa-402a-8afa-908d.jpg