posted 10 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 49,
Visits: 486
Made my second mould yesterday, but it did not turn out as good as the first one.
Is this mould fixable?
How do I fix the bubble holes? And how do I get the release tape out of the mould?
Reply
Like
3
Reply
carbonfibreworks
carbonfibreworks
posted 10 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 292,
Visits: 4.5K
Hi Redrocket
You can mix some gel coat and use it to fill the voids then flat back with some fine paper and polish and you should be able to remove the release tape with a sharp blade/ scalpel .
Regards Chris
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
How do I fix this mould?
67redrocket
-
10 Years Ago
Hi Redrocket You can mix some gel coat and use it to fill the voids then flat back with some fine...
carbonfibreworks
-
10 Years Ago
Post Reply
Like
3
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search