Made my second mould yesterday, but it did not turn out as good as the first one.

Is this mould fixable? 

How do I fix the bubble holes? And how do I get the release tape out of the mould?

http://www.talkcomposites.com/Uploads/Images/d4faf592-c2aa-402a-8afa-908d.jpg