Hello Guys

Can anyone recomend a spray tack for epoxy resin infusion ?

I Infused a part on the weekend using Infuzene and it left stringy marks on the surface. Maybe i used to much but it sprays so inconsistently , hard to get only a mist.

I live in Australia so any local help with suppliers would be great.

Thanks

Rod.
Replies
rallyfly
rallyfly
Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)Supreme Being (157 reputation)
Group: Forum Members
Posts: 25, Visits: 85
Well no luck with the Aerofix 3    Elite Composites are currently looking for an aternative.

I used some 3m super 75 repositionable , mist coat on the cloth , worked great. just a slight stickyness on the part easily removed with wax and grease remover.  surface perfect !
ChrisR
ChrisR
Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)Supreme Being (2.8K reputation)
Group: Forum Members
Posts: 363, Visits: 3K
Warren posted up a neat spray tack alternative not long ago, haven't tried it myself as I have a supply of aerofix3 but may do in the future
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
MarkMK - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
Hanaldo - 10 Years Ago
rallyfly - 10 Years Ago
ChrisR - 10 Years Ago
rallyfly - 10 Years Ago
Warren (Staff) - 10 Years Ago
Chris Scott - 10 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search